John@barewood
J
John@barewood
posted 6 Years Ago
ANSWER
HOT
Topic Details
J
Group: Forum Members
Posts: 3,
Visits: 6
Hello all,
Ive been using CC10/50 for about a year now and recently been experiencing small micro bubbles appearing in my pours. CC 10/50 1kg pack has been laying for some time and developed crystallizing at the bottom.
Ive put it in hot water and let it cool naturally and got it back to a nice clear consistency.
Mixing approx 90g in 2:1 ratio
Mixing in small plastic cups for 3mins then pour in to second cup with further 1 min mix.
poured in to 3rd cup slowly at a depth of 35mm
used heat gun to pop top bubbles
left to cure over night
any help would be greatly received, thanks
in the morning i can see tiny bubbles thru the entire 35mm depth of the pour
Reply
Like
4
Reply
Mark59
M
Mark59
posted 6 Years Ago
ANSWER
HOT
Post Details
M
Group: Forum Members
Posts: 3,
Visits: 23
Hi
I've been having the same issues.
Is there an update from John as to using a new un-opened product?
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
micro bubbles in Clearcast 10/50
John@barewood
-
6 Years Ago
Hi John, Can I just check; is this GlassCast (You've put Clear Cast) so want to ensure we're talking about the same product; if so, the mix ratio when mixing by weight is 100:45 rather than 2:1, the....
Rich (Staff)
-
6 Years Ago
Update** Taking the above advice, I slowly heated parts A+B to around 25 Degree C and maintained this room temp for the pour and set. This time correctly measuring weight ratio @ 100:45. Mixed for 3....
John@barewood
-
6 Years Ago
Strange, normally we would expect it to be as per the bottom block, especially if you heat gunned it. A few microbubbles would be normal in a resin that has not been degassed, although they would onl...
Warren (Staff)
-
6 Years Ago
So I did another pour, following the procedure as before, nice warm Part A & B in a warm room 22 Deg C. As I poured slowly, I used a heat gun, so pour about 5mm then used heat gun. In total I poured....
john lyons
-
6 Years Ago
Very strange. Certainly not something we have seen with new bubbles forming after degassing unless there is moisture present. Would certainly be interesting to see more feedback from the new batch......
Warren (Staff)
-
6 Years Ago
Hi I've been having the same issues. Is there an update from John as to using a new un-opened product?
Mark59
-
6 Years Ago
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search