By John@barewood - 1/10/2019 8:18:34 AM
Hello all, Ive been using CC10/50 for about a year now and recently been experiencing small micro bubbles appearing in my pours. CC 10/50 1kg pack has been laying for some time and developed crystallizing at the bottom. Ive put it in hot water and let it cool naturally and got it back to a nice clear consistency. Mixing approx 90g in 2:1 ratio Mixing in small plastic cups for 3mins then pour in to second cup with further 1 min mix. poured in to 3rd cup slowly at a depth of 35mm used heat gun to pop top bubbles left to cure over night any help would be greatly received, thanks
 in the morning i can see tiny bubbles thru the entire 35mm depth of the pour
|
By Mark59 - 4/5/2019 8:19:22 AM
Hi
I've been having the same issues.
Is there an update from John as to using a new un-opened product?
|
|