Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
Very strange. Certainly not something we have seen with new bubbles forming after degassing unless there is moisture present. Would certainly be interesting to see more feedback from the new batch. There may well be some deteriation or factor we have yet to see with very old batches.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|