+x Frank - 12/26/2018 12:32:43 PM@Hanaldo: With the next Part I will try to degas the resin-chopped-strand-mix.@ George Sychrovsky :Yes, it would be the best way, to build a new mould and to design the mould for parts made of reinforced resin. But the mould is already made the way it is. And I already produced a useable Part in it. So, the job is done and the bike has its Carbon-Front-Fender made of CF looking nice.I do not want to build a complete new mould. Perhaps I can change the mould-part that is made from polyurethane. 1) I probably can design it to leave a flat area in the mounting-section of the Front-fender, to which I can bond an angle and the tubes made of CF. 2) Another way would probably be, to drill a hole in the PU-Mouldpart, pull the Vacuum through this hole and feed the resin from both small ends of the mould.@oekmont: Next time I will try to bring more reinforcement into the mounting-section and degas it.@f1rob: I agree to this. I just copied the part. Perhaps option 2) can help with that.I have to think about it.RegardsFrank