Group: Forum Members
Posts: 2.5K,
Visits: 28K
|
Well, perhaps. But I would suggest switching to a more advanced process, like resin infusion or pre-preg. Or at the very least, wet-lay vacuum bagging. You really need some sort of consolidation to hold things in place while the resin cures. Wet-lay vacuum bagging may be slightly cheaper, but it does also require a good amount of skill to get a good result. Resin infusion and pre-preg are much more forgiving, but more expensive processes.
|