Barnsley-Bill
B
Barnsley-Bill
posted 7 Years Ago
ANSWER
HOT
Topic Details
B
Group: Forum Members
Posts: 25,
Visits: 489
I wrote the heat ramp i want to use in the parameters 60c for 10 hours 70c for 2 hours 80c for 2 hours 90 for 2 hours to cure my mould and can't find how to start the oven ? ' do I need to set the ctrl. method in the control to something else ? thanks I've finally built my oven and connected it to my spare laptop .
Thanks
Reply
Like
3
Reply
Barnsley-Bill
B
Barnsley-Bill
posted 7 Years Ago
ANSWER
HOT
Post Details
B
Group: Forum Members
Posts: 25,
Visits: 489
could you tell me how to do it manually as I want to learn this way as well please.
thanks.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
starting my curing oven using a laptop
Barnsley-Bill
-
7 Years Ago
On-off will simply ramp up to the set value, it won't run a program. Change the control method to Prog to run programmed ramp rates and dwells. However, this shouldn't actually stop the oven from...
Hanaldo
-
7 Years Ago
sorted it mate thanks I must have slackend a wire when fitting the wires for the usb adapter.
Barnsley-Bill
-
7 Years Ago
could you tell me how to do it manually as I want to learn this way as well please. thanks.
Barnsley-Bill
-
7 Years Ago
Hard to explain without writing a novel to rival The Hobbit. Your controller should have come with a manual? If not, it is available online if you Google Omega CN7800 Manual. It's a bit hard to make....
Hanaldo
-
7 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search