By Barnsley-Bill - 11/4/2018 2:00:29 PM

  

I wrote the heat ramp i want to use in the parameters 60c for 10 hours 70c for 2 hours 80c for 2 hours 90 for 2 hours to cure my mould and can't find how to start the oven ? ' do I need to set the ctrl. method in the control to something else ? thanks I've finally built my oven  and connected it to my spare laptop .
Thanks
By Hanaldo - 11/5/2018 12:17:26 AM