Has anyone had experience with their catch pot lid cracking during normal use? It wasn't cracked when I set up my system for infusion but after I left it overnight and came back, I have two rather serious cracks in the lid which also caused me to lose vacuum entirely.
Reply
d3ntr0n
d
Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)Forum Guru (63 reputation)
Group: Forum Members
Posts: 10, Visits: 94
Hanaldo - 10/9/2018 4:18:10 AM
Definitely strange. Is it an Easy Composites catch can? Has the acrylic been exposed to any solvents like acetone?

It apparently is a QC issue from the vendor. No, it wasn't from Easy Composites, but I just contacted the vendor and they said it has been known to happen to that product. They sent us a new lid free of charge. Thank you for your response!