Has anyone had experience with their catch pot lid cracking during normal use? It wasn't cracked when I set up my system for infusion but after I left it overnight and came back, I have two rather serious cracks in the lid which also caused me to lose vacuum entirely.
Hanaldo
Hanaldo
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Definitely strange. Is it an Easy Composites catch can? Has the acrylic been exposed to any solvents like acetone?
d3ntr0n
d
Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)Supreme Being (107 reputation)
Group: Forum Members
Posts: 10, Visits: 94
Hanaldo - 10/9/2018 4:18:10 AM
Definitely strange. Is it an Easy Composites catch can? Has the acrylic been exposed to any solvents like acetone?

It apparently is a QC issue from the vendor. No, it wasn't from Easy Composites, but I just contacted the vendor and they said it has been known to happen to that product. They sent us a new lid free of charge. Thank you for your response!