Rob is talking high end F1 applications, so using pre-pregs. If your max Tg is 90 then you dont want to take it up to 160.
Acetone is commonly used for this 'lost core' sort of application, however immersing epoxy in acetone isn't really ideal. If it is the only way, then it probably wont suffer TOO much with only an hour, but I would want to make sure the epoxy is thoroughly cured - which realistically means giving it a post-cure up to your max Tg.
|