You can measure the catalyst by weight or volume as the density is 1g/cm3. Often it is more convenient to have an MEKP dispenser bottle or syringe which has fine volume graduations on it than trying to weigh out the catalyst. So in this case, you would weight out the primer and add the correct volume of MEKP from the dispenser bottle.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|