			            The carbon Rod uses an epoxy matrix that has a HDT of 75C.  This is the same for all our pultrusion’s as they are all now sourced in epoxy. 600C would need a very specialist resin and I am not aware of any rods or similar sections made from carbon with a suitable HDT.                  
			            
  				