By DeanOxley - 6/27/2018 9:44:21 AM
I was just wondering what kind of temperature can your carbon fibre rods withstand? Looking to go up in excess of 600 degrees.
|
By Warren (Staff) - 6/27/2018 11:56:05 AM
The carbon Rod uses an epoxy matrix that has a HDT of 75C. This is the same for all our pultrusion’s as they are all now sourced in epoxy. 600C would need a very specialist resin and I am not aware of any rods or similar sections made from carbon with a suitable HDT.
|
|