Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - Product Specific Pages
»
Carbon Fibre Tube and Section
»
Carbon Fibre Temperature
Carbon Fibre Temperature
Post Reply
Like
6
Carbon Fibre Temperature
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
DeanOxley
D
DeanOxley
posted 8 Years Ago
ANSWER
HOT
Topic Details
D
Group: Forum Members
Posts: 1,
Visits: 2
I was just wondering what kind of temperature can your carbon fibre rods withstand? Looking to go up in excess of 600 degrees.
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Carbon Fibre Temperature
DeanOxley
-
8 Years Ago
The carbon Rod uses an epoxy matrix that has a HDT of 75C. This is the same for all our pultrusion’s as they are all now sourced in epoxy. 600C would need a very specialist resin and I am not aware....
Warren (Staff)
-
8 Years Ago
Post Reply
Like
6
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search