Group: Forum Members
Posts: 15,
Visits: 28
|
I dented my factory metal heat shield on my KX 450F and want to create a similar one out of carbon. I've made lots of carbon bits over the days but never a part that bolts directly to a high heat part. Temps reach 400F at the exhaust flange and the pipe bends and at about 12 inches from the flange is where the burn/heat guard mounts. For temps that would be likely around 350F, which resin should I use?
Mike
|