I dented my factory metal heat shield on my KX 450F and want to create a similar one out of carbon. I've made lots of carbon bits over the days but never a part that bolts directly to a high heat part. Temps reach 400F at the exhaust flange and the pipe bends and at about 12 inches from the flange is where the burn/heat guard mounts. For temps that would be likely around 350F, which resin should I use?

Mike
TWINFOX
TWINFOX
Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)Junior Member (21 reputation)
Group: Forum Members
Posts: 3, Visits: 190
Hello Mike

I've did it this way: The carbon part was made with a standard epoxy resin thats heat resistand up to130°C. To get a better heat protection, I've bondet a heat protection on the inner side. As a heat protection you can use aluminium foil tape or an aluminium shieldet fibre glass. Both products can be found on any local motorsport parts dealer.

Dirk



Regards 
Dirk

Warren
Warren
Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)
Group: Administrators
Posts: 214, Visits: 782
you can get a slightly higher temp resin from EC here.  However i would agree with twinfox that realistically youd want a heat reflective barrier on the inside.  Especially if its for cosmetic reasons.

make sure the part is fully cured either during the process in an oven or using a post cure process as otherwise you will find it may go soft under high heat until it really is fully chemically cured throughout.