Motorcycle exhaust heat shield
Motorcycle exhaust heat shield
Post Reply
Like
3
Motorcycle exhaust heat shield
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
mwr2452
mwr2452
posted 13 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 15,
Visits: 28
I dented my factory metal heat shield on my KX 450F and want to create a similar one out of carbon. I've made lots of carbon bits over the days but never a part that bolts directly to a high heat part. Temps reach 400F at the exhaust flange and the pipe bends and at about 12 inches from the flange is where the burn/heat guard mounts. For temps that would be likely around 350F, which resin should I use?
Mike
Reply
Like
3
TWINFOX
TWINFOX
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 3,
Visits: 190
Hello Mike
I've did it this way: The carbon part was made with a standard epoxy resin thats heat resistand up to130°C. To get a better heat protection, I've bondet a heat protection on the inner side. As a heat protection you can use aluminium foil tape or an aluminium shieldet fibre glass. Both products can be found on any local motorsport parts dealer.
Dirk
Regards 
Dirk
TWINFOX
Reply
Like
3
Warren
Warren
posted 13 Years Ago
ANSWER
HOT
Post Details
Group: Administrators
Posts: 214,
Visits: 782
you can get a slightly higher temp resin from EC
here
. However i would agree with twinfox that realistically youd want a heat reflective barrier on the inside. Especially if its for cosmetic reasons.
make sure the part is fully cured either during the process in an oven or using a post cure process as otherwise you will find it may go soft under high heat until it really is fully chemically cured throughout.
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search