I'm tired of doing wet lay up for this, it's time to bag it.

Bearing mind that there is a "high point", where would be best to put the spiral? along one end and up to that high point? Or something else?  Would it need more layers of infusion mesh on the high "sides"? Any direction you guys could give would be appreciated.  I know that the flanges aren't large so I'd have to envelope bag the whole thing.

The reinforcement is 4 layers of 200 carbon if that makes a difference (the marks on the mould are just stray bits of peel ply that drifted on to it)

http://www.defender2.net/gallery/albums/userpics/11127/mould.jpg
Edited 13 Years Ago by mikew
Replies
mikew
mikew
Supreme Being (452 reputation)Supreme Being (452 reputation)Supreme Being (452 reputation)Supreme Being (452 reputation)Supreme Being (452 reputation)Supreme Being (452 reputation)Supreme Being (452 reputation)Supreme Being (452 reputation)Supreme Being (452 reputation)
Group: Forum Members
Posts: 56, Visits: 128
Thanks both. Putting the vac line in the middle, would that not mean that resin would be pulled out pretty fast before the ends of the part were wetted out? Side to side it's obviously a lot narrower...

Joe, that might be an idea, yes, though I have quite a bit of 200 carbon which is mostly offcuts a friend gave me and the weave is a little "pulled" so I'm using that for the mid layers. Once I run out though, I'll go with your suggestion if I need to make more. Thanks.
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
i'm not trying to spam this forum with my videos but this can give you an idea, Its quit "similar" to you project.
put the resininlet as much in the middle as possible and vacuumexit in the spiral around the mould.

check video, you can skip untill 6min if you want Wink there you can see the setup and infusion after it.
good luck Wink 

of topic, helmet is almost done, working on a template for painting now and clearcoat and it's done Smile



Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com