	Group: Forum Members 	        
    Posts: 56, 
    Visits: 128 
    
 
          
		     | 
				                       
                 
                
                    
			            Thanks both. Putting the vac line in the middle, would that not mean that resin would be pulled out pretty fast before the ends of the part were wetted out? Side to side it's obviously a lot narrower...
  Joe, that might be an idea, yes, though I have quite a bit of 200 carbon which is mostly offcuts a friend gave me and the weave is a little "pulled" so I'm using that for the mid layers. Once I run out though, I'll go with your suggestion if I need to make more. Thanks.                
			            				
			                                 
                     
                                            
                         
                    
                  
             |