Hello friends,

I was studying making 3D impression moulds and sealing with epoxy resin to make carbon fiber parts in the Wet Layup + Vacuum Bagging or Vacuum infusion process. 

Has anyone done any 3D impression mould?
What better material for printing?

The composites will be cured at room temperature.

Thanks!
Reply
Dezer
Dezer
Supreme Being (694 reputation)Supreme Being (694 reputation)Supreme Being (694 reputation)Supreme Being (694 reputation)Supreme Being (694 reputation)Supreme Being (694 reputation)Supreme Being (694 reputation)Supreme Being (694 reputation)Supreme Being (694 reputation)
Group: Forum Members
Posts: 74, Visits: 1.8K
scottracing - 5/16/2018 7:38:05 AM
ive done plenty of 3d printed tooling, if you are doing room temp wet lay then you can get away with PLA printed materials but you need to make sure they are properly sealed and released as Epoxy resins stick to them really well. Plus there will be a bit of wet sanding to get them smooth, or you can cover them in flash tape or PTFE release film like Tygaflor

If you are looking into elevated temperatures or autoclave curing then you really need to be looking at better engineered materials, have a look at the graphite am website and there range of ceramic and carbon printed materials.
I would also investigate the use of stratasys ULTEM 1010 and 9085 materials as they are suitable for high temp and autoclave curing.


Thanks Scottracing, 

As it will be cured by ambient temperature the conventional materials will supply my needs well.

Do you have any pictures of a 3D printed mould ?
Thankful.

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Dezer - 7 Years Ago
scottracing - 7 Years Ago
Dezer - 7 Years Ago
SleepingAwake - 7 Years Ago
Dezer - 7 Years Ago
vieteejais - 5 Years Ago
scottracing - 7 Years Ago
SleepingAwake - 7 Years Ago
KostasBiz - 7 Years Ago
                     Many. But it's not like I was watching it...
SleepingAwake - 7 Years Ago
Warren (Staff) - 7 Years Ago
scottracing - 7 Years Ago
KostasBiz - 7 Years Ago
SleepingAwake - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search