Carbon Fiber Layup with Mould 3D Printer


Author
Message
Dezer
Dezer
Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)
Group: Forum Members
Posts: 74, Visits: 1.8K
Hello friends,

I was studying making 3D impression moulds and sealing with epoxy resin to make carbon fiber parts in the Wet Layup + Vacuum Bagging or Vacuum infusion process. 

Has anyone done any 3D impression mould?
What better material for printing?

The composites will be cured at room temperature.

Thanks!
scottracing
scottracing
Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
ive done plenty of 3d printed tooling, if you are doing room temp wet lay then you can get away with PLA printed materials but you need to make sure they are properly sealed and released as Epoxy resins stick to them really well. Plus there will be a bit of wet sanding to get them smooth, or you can cover them in flash tape or PTFE release film like Tygaflor

If you are looking into elevated temperatures or autoclave curing then you really need to be looking at better engineered materials, have a look at the graphite am website and there range of ceramic and carbon printed materials.
I would also investigate the use of stratasys ULTEM 1010 and 9085 materials as they are suitable for high temp and autoclave curing.


Dezer
Dezer
Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)
Group: Forum Members
Posts: 74, Visits: 1.8K
scottracing - 5/16/2018 7:38:05 AM
ive done plenty of 3d printed tooling, if you are doing room temp wet lay then you can get away with PLA printed materials but you need to make sure they are properly sealed and released as Epoxy resins stick to them really well. Plus there will be a bit of wet sanding to get them smooth, or you can cover them in flash tape or PTFE release film like Tygaflor

If you are looking into elevated temperatures or autoclave curing then you really need to be looking at better engineered materials, have a look at the graphite am website and there range of ceramic and carbon printed materials.
I would also investigate the use of stratasys ULTEM 1010 and 9085 materials as they are suitable for high temp and autoclave curing.


Thanks Scottracing, 

As it will be cured by ambient temperature the conventional materials will supply my needs well.

Do you have any pictures of a 3D printed mould ?
Thankful.

Lester Populaire
L
Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
I just have some pictures of printed positive moulds on hand and thought i would share them. printed in PLA on a Prusa printer.


second layer of spray filler


sanded to 800 grid


with tooling gel coat


finished mould (made with vacuum infusion) and the first part


first part close up. Finish straight out of the mould.


Another project with the bar and the lower mould have printed to get an accurate split line exactly in the center of the bar.


this is how the first mould have is made, then the lower part is removed and a composite mould is made instead.


And a close up of the finish. getting a really smooth finish and decent dimensional accuracy is really easy even with a relatively big layer height.

I hope this helps.
Cheers, Reto






Dezer
Dezer
Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)Supreme Being (1.1K reputation)
Group: Forum Members
Posts: 74, Visits: 1.8K
SleepingAwake - 5/19/2018 8:06:17 AM
I just have some pictures of printed positive moulds on hand and thought i would share them. printed in PLA on a Prusa printer.


second layer of spray filler


sanded to 800 grid


with tooling gel coat


finished mould (made with vacuum infusion) and the first part


first part close up. Finish straight out of the mould.


Another project with the bar and the lower mould have printed to get an accurate split line exactly in the center of the bar.


this is how the first mould have is made, then the lower part is removed and a composite mould is made instead.


And a close up of the finish. getting a really smooth finish and decent dimensional accuracy is really easy even with a relatively big layer height.

I hope this helps.
Cheers, Reto







This will help me a lot, for sure!

Many thanks friend!
scottracing
scottracing
Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
what layer height did you use on the PLA print? And did you sand it prior to the first coat of primer?

The finished part looks brilliant, is that a flax/hemp material you made the part from?

Lester Populaire
L
Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)Supreme Being (4.5K reputation)
Group: Forum Members
Posts: 311, Visits: 13K
scottracing - 5/30/2018 11:14:56 AM
what layer height did you use on the PLA print? And did you sand it prior to the first coat of primer?

The finished part looks brilliant, is that a flax/hemp material you made the part from?

I usually print with a Layer height of 0.15 to 0.2mm and give it a light sand to get rid of small bumps where a new layer started and any things like that. Then usually two coats of heavy filler and one coat of finishing filler with wet sanding is enough to get a good finish.

The part is made from Bcomp's ampliTex 5040 fabric.

Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Nice to see some natural fibres being used.  How does it compare stiffness wise?  Most natural fibres seem very poor compared to more advanced composite fibres - albeit usually the environmental credentials or different looks are usually more of a priority.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
scottracing
scottracing
Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
looks really good,we have been trialling some of the bcomp material at work and finding its not as good as it says on the tin,but i think for non structural applications like bodywork it should be good,i especially like the power ribs such a great and simple idea


KOSTAS
KOSTAS
Supreme Being (489 reputation)Supreme Being (489 reputation)Supreme Being (489 reputation)Supreme Being (489 reputation)Supreme Being (489 reputation)Supreme Being (489 reputation)Supreme Being (489 reputation)Supreme Being (489 reputation)Supreme Being (489 reputation)
Group: Forum Members
Posts: 30, Visits: 244
Lester Populaire - 5/30/2018 9:24:47 PM
scottracing - 5/30/2018 11:14:56 AM
what layer height did you use on the PLA print? And did you sand it prior to the first coat of primer?

The finished part looks brilliant, is that a flax/hemp material you made the part from?

I usually print with a Layer height of 0.15 to 0.2mm and give it a light sand to get rid of small bumps where a new layer started and any things like that. Then usually two coats of heavy filler and one coat of finishing filler with wet sanding is enough to get a good finish.

The part is made from Bcomp's ampliTex 5040 fabric.


0.15 layer height !!!! How many hours did it take you  to print this bar mold ?

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search