Resin infusion from Steel Mould


Author
Message
Assaltofrontale
Assaltofrontale
Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)Junior Member (10 reputation)
Group: Forum Members
Posts: 2, Visits: 12
Hello to everyone,
I'm new of this forum and newbie about infusion.
I have some questions:
- Is it possible to use a steel mould (zink finished or black e-coated) to create pieces with resin infusion?
- Which Mould Release Agent do I have to use?

Thanks

Replies
neilb
neilb
Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)Supreme Being (764 reputation)
Group: Forum Members
Posts: 107, Visits: 504
steel moulds i would say are the pinnacle of moulds especially for mass production of quality parts.

as for release agent, you don't have to use any particular one but chemical agents are better than pva. pva has its place but its like carbs on a car, they work but they have had there day. wax and a product called ease lease is the preferred choice i would say
fgayford
fgayford
Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
neilb (03/09/2012)
steel moulds i would say are the pinnacle of moulds especially for mass production of quality parts.

as for release agent, you don't have to use any particular one but chemical agents are better than pva. pva has its place but its like carbs on a car, they work but they have had there day. wax and a product called ease lease is the preferred choice i would say


Just watch out that the chemical release does not contain silicone, which will bite you if you try to paint it later. You will get fisheyes.

Fred 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search