What do I need to make a complete set of custom carbon fibre panels for my project car?


What do I need to make a complete set of custom carbon fibre panels for my project car?
Author
Message
garyH
garyH
Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)Forum Guru (72 reputation)
Group: Forum Members
Posts: 2, Visits: 5
Hi,

Basically im wanting to build a crazy v8 mk2 mr2 with custom body kit, front and rear clam type boot/bonnet, slightly lengthened and a tad wider.. can you advice me on the type of carbon fibre would be best suited for looks and light weight? how much carbon fibre would be needed to do a pretty much an entire outer shell? also wanting to custom engine parts / inlet etc and a carbon dash... i've done alot with fibre glass but i think my project needs to be carbon as im wanting to show it on completion, advice on materials and prices would be great.

Thanks

Gary
Edited 13 Years Ago by garyH
Replies
Sawrel
Sawrel
Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)
Group: Forum Members
Posts: 6, Visits: 49
Thank you very much for your reply. It is very helpful.

One more question:

At one topic on the forum I saw the equation to
how many I  needed epoxy Infusion Resin to comply with an object, but unfortunately I can not find it now. Can I ask to enter it in this thread.

Thank you very much.

Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)Composites Expert (Staff) (8.4K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Follow this link to Paul's Resin Infusion Resin Usage Calculation.

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
garyH - 14 Years Ago
Matt (Staff) - 14 Years Ago
garyH - 14 Years Ago
Matt (Staff) - 14 Years Ago
Carbon Tuner - 13 Years Ago
Volvofan - 13 Years Ago
Matt (Staff) - 13 Years Ago
Volvofan - 13 Years Ago
Nate - 13 Years Ago
Sawrel - 13 Years Ago
Matt (Staff) - 13 Years Ago
Sawrel - 13 Years Ago
Matt (Staff) - 13 Years Ago
baja_patient - 13 Years Ago
Sawrel - 13 Years Ago
Matt (Staff) - 13 Years Ago
Sawrel - 13 Years Ago
Sawrel - 13 Years Ago
dei - 12 Years Ago
Warren (Staff) - 12 Years Ago
dei - 12 Years Ago
andygtt - 12 Years Ago
20_rc51_00 - 11 Years Ago
Warren (Staff) - 10 Years Ago
jaffa - 10 Years Ago
Warren (Staff) - 10 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search