Hello everyone,
I am trying to understand why carbon fiber components in BMW 7 series and many other cars are used in conjunction with Steel? Why are carbon fiber stand-alone components not used instead of these hybrids? Are there any intrinsic problems with stand-alone carbon fiber components? 
Edited 7 Years Ago by Siddu
Reply
f1rob
f1rob
Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)Supreme Being (2K reputation)
Group: Forum Members
Posts: 237, Visits: 4.8K
A f1 tub and a nose are grey specific in their design that they have to pass 1 set of rules in a very specific crash test and the squeeze tests.
Lots of " cheats" that go on
8.1 Ali core used for example in the squeeze area.
You could never make a hole tub with it but easy to put in your test points
Your nose,the very front is cosmetic as it will be destroyed in a nano second so people don't bother doing a structural build to the tip
Not unknown for wing fixing inserts to be missed out in a crash box.
In a crash test solid carbon or Ali inserts can plod through core like a snow plod
You have to crash within the deceleration curve so if you took a cross section of a nose you would see varying thickness laminate.
The same with core and differing densitys 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Siddu - 7 Years Ago
Hanaldo - 7 Years Ago
Siddu - 7 Years Ago
oekmont - 7 Years Ago
Siddu - 7 Years Ago
oekmont - 7 Years Ago
f1rob - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search