GC50 double gel and bonding


Author
Message
Kurt Halkier
Kurt Halkier
Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)Supreme Being (90 reputation)
Group: Forum Members
Posts: 3, Visits: 9
We want to make two layers of GC50 onto our mold, but you do not recommend this, as GC50 will NOT bond to itself leading to delamination.!
But it is possible if done before the first layer of gelcoat has completely hardened. 
The reason is that we want to 
use a colored GC50 sprayed onto the mold via a template, and then spraying a GC50 with another color on the rest of moldbefore final IN2 infusion.

Warren (Staff)
Warren (Staff)
Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)Supreme Being (36K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Unfortunately it will not bond properly.  It only bonds to itself when it is totally wet which would not be suitable for your needs as the colours would blend.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Almand
Almand
Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)
Group: Forum Members
Posts: 19, Visits: 108
Warren (Staff) - 4/12/2018 8:30:13 AM
Unfortunately it will not bond properly.  It only bonds to itself when it is totally wet which would not be suitable for your needs as the colours would blend.

Hi Warren, do you know another process/methode/product we can use instead, if we want to have more than one gelcoat color or clear gelcoat. We want to apply it direct by spraying it in mould prepaired with Easy Release agent.
Best regards 
Keld and Kurt
oekmont
oekmont
Supreme Being (7.8K reputation)Supreme Being (7.8K reputation)Supreme Being (7.8K reputation)Supreme Being (7.8K reputation)Supreme Being (7.8K reputation)Supreme Being (7.8K reputation)Supreme Being (7.8K reputation)Supreme Being (7.8K reputation)Supreme Being (7.8K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
Search for inmould coating laquer. It is exactly made for this applications.