By Kurt Halkier - 4/12/2018 6:30:56 AM
We want to make two layers of GC50 onto our mold, but you do not recommend this, as GC50 will NOT bond to itself leading to delamination.! But it is possible if done before the first layer of gelcoat has completely hardened. The reason is that we want to use a colored GC50 sprayed onto the mold via a template, and then spraying a GC50 with another color on the rest of moldbefore final IN2 infusion.
|
By oekmont - 4/15/2018 6:30:17 AM
Search for inmould coating laquer. It is exactly made for this applications.
|
|