shelf life relase agent and wax additive solution MW


Author
Message
Adelbolide
Adelbolide
Supreme Being (149 reputation)Supreme Being (149 reputation)Supreme Being (149 reputation)Supreme Being (149 reputation)Supreme Being (149 reputation)Supreme Being (149 reputation)Supreme Being (149 reputation)Supreme Being (149 reputation)Supreme Being (149 reputation)
Group: Forum Members
Posts: 16, Visits: 112
Hello,
is there a shelf life for release agents and wax additive solution MW. I'm having some problems with this products. Recently I used a release agent I've opened some time ago (1 year) and it didn't work very well.

I've also a wax additive I bought 6 months ago. I opened it only now and the product became solid.

Is there a shelf life for this products? A best use date after opening?

Thanks in advance
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Very strange that the wax solution has dried out. I've got a bottle of wax solution here that is about 7 years old, I still use it every now and then. Using it today in fact!