EasyLease has a shelf life of one year max. The more you open the bottle, the more it is likely to reduce the life span as the mixture is hydroscopic so will absorb moisture from the air which will degrade its performance. Certainly over a year I would be considering a replacement.
The wax additive sounds like it has dried out. - try and ensure the lid is fully sealed after use. You may find it is just on the surface in which case break the wax up and remix and you might be able to use it if there are no bits in it.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|