Ideally you need a pump that can get as close to full vacuum as possible to something like 29.9 in hg or similar. At that level the resin should degas fine.
Also be aware that P6 is quite moisture sensitive so this time of year some of the extra bubbles could be due to the moisture causing a reaction so try and take care of your working environment.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|