Hi there

I’m not having a lot of success degassing P6 two part resin.. is there a particular negative pressure I need to achieve?

I’m wondering if the pump I’m using hasn’t got enough oomph!

Though it works fine for the silicon mould making part of the process?

Your thoughts would be appreciated!

Thanks

Ben