Group: Forum Members
Posts: 107,
Visits: 504
|
i may have missed this but have you isolated the catch pot entirely? ie, pulled a vacuum then clamped off both lines and not just relied on the valve on the pump?
also just looking back at the pics have you fitted the valve on the pump and the barb conector with PTFE tape?
|