Hi guys what would you use to take a mould of a car Dash, because it's like a vinyl cover on there in guessing epoxy ect would eat in to it? 
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
PVA coat it if you are worried about the Epoxy eating into it.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant