I have moulded 50 dashes of an old volkswagen dash.
The moulds are silicone surface supported by fibreglass backing mould. This is the body moulding type silicone so it is harmless and easy to release without any risk of damage.
The parts are polyurethane resin/foam and have a similar touch and feel to the original dashes.






Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
PVA coat it if you are worried about the Epoxy eating into it.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
111mattin111
111mattin111
Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)Supreme Being (449 reputation)
Group: Forum Members
Posts: 67, Visits: 910
Hi guys what would you use to take a mould of a car Dash, because it's like a vinyl cover on there in guessing epoxy ect would eat in to it? 