By 111mattin111 - 2/26/2018 10:57:54 AM
Hi guys what would you use to take a mould of a car Dash, because it's like a vinyl cover on there in guessing epoxy ect would eat in to it?
|
By Fasta - 2/27/2018 1:12:38 AM
I have moulded 50 dashes of an old volkswagen dash. The moulds are silicone surface supported by fibreglass backing mould. This is the body moulding type silicone so it is harmless and easy to release without any risk of damage. The parts are polyurethane resin/foam and have a similar touch and feel to the original dashes.

|
|