Group: Administrators
Posts: 2.5K,
Visits: 8.5K
|
If the surface of the mould is gloss, then the part will come out gloss. is the original pattern a plaster cast or similar? If so you could sand the surface to get an even finish then mould from that and you should get that finish on the casting which will give the frosted type appearance.
Warren Penalver Easy Composites / Carbon Mods - Technical Support Assistant
|