Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Resin Casting and Moulding Forum
»
Share your Casting Project
»
how to make frosted glass effect in resin
how to make frosted glass effect in resin
Post Reply
Like
8
how to make frosted glass effect in resin
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Patrycja
P
Patrycja
posted 8 Years Ago
ANSWER
HOT
Topic Details
P
Group: Forum Members
Posts: 1,
Visits: 9
Hi guys
I really need your help, Im just started using clear polyester resin for the first time and I love it
But Im trying to get frosted glass effect in my baby feet casting project and I have no idea how to make it
I bought clear polyester casting resin, translucent tinting pigments, addition cure silicone rubber.
I try couple times but my baby feet casting came out in some parts frosted but most of it shiny
please can someone explain me what I'm doing wrong ?how to make this effect ?
what is the best resin to use to make frosted effect?
what is the best rubber to use for moulds ?
Edited
8 Years Ago by
Patrycja
Reply
Like
8
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
how to make frosted glass effect in resin
Patrycja
-
8 Years Ago
If the surface of the mould is gloss, then the part will come out gloss. is the original pattern a plaster cast or similar? If so you could sand the surface to get an even finish then mould from that...
Warren (Staff)
-
8 Years Ago
Post Reply
Like
8
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search