Hello,
I am new to composites. I have started with few sets from Easy Composites.

I made a few tests on plexiglass and unfortunately I do not get a glossy surface on the carbon plate. In addition after 24hrs the resin did not fully cure and the plates are a bit soft Smile

Please see the pictures. 

I applied Easy Release Agent 2 times. 1 application and then after 5 minutes the second one. The ration resin to hardener was 100:30. (Slow)

Can you please advice
1) What can be wrong?
2) How many applications should I do with Easy Release and what should be the time in between?


Thank you!

Edited 7 Years Ago by CMax
Reply
CMax
C
Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)Forum Guru (69 reputation)
Group: Forum Members
Posts: 9, Visits: 38
Cool. Understood! Thank you so much for support!
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
CMax - 7 Years Ago
Warren (Staff) - 7 Years Ago
CMax - 7 Years Ago
CMax - 7 Years Ago
oekmont - 7 Years Ago
CMax - 7 Years Ago
Warren (Staff) - 7 Years Ago
CMax - 7 Years Ago
Warren (Staff) - 7 Years Ago
oekmont - 7 Years Ago
CMax - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search