By CMax - 1/30/2018 10:49:15 PM
Hello, I am new to composites. I have started with few sets from Easy Composites.
I made a few tests on plexiglass and unfortunately I do not get a glossy surface on the carbon plate. In addition after 24hrs the resin did not fully cure and the plates are a bit soft 
Please see the pictures.
I applied Easy Release Agent 2 times. 1 application and then after 5 minutes the second one. The ration resin to hardener was 100:30. (Slow)
Can you please advice 1) What can be wrong? 2) How many applications should I do with Easy Release and what should be the time in between?
 
Thank you!
|
By CMax - 2/5/2018 11:49:15 AM
Cool. Understood! Thank you so much for support!
|
|