Hi, I intend to build a Carbon/Kevlar Roof for an UTV. The dimensions are 1,0m. x 1,3m. , I need to have a strength similar to that of an aluminum plate of 5mm. thickness (it's a flat plate with the first 15cm. folded at 30 degrees)
I'm thinking of build the piece by infusion.
What do you advise me? - thickness of the laminate; number of layers of material; do I use only Carbon Kevlar 2/2 Twill or Carbon Black Twaron layers, or should I insert some layers of Carbon fibre Biaxial, etc... 
I thank you for any help.

José Moleiro

Warren (Staff)
Warren (Staff)
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
A 5mm thick roof of solid laminate would be quite heavy.  You might want to consider the use of a structural core, such as 3mm Lantor Soric or 3D core.  Both are easy to infuse and will help product a stiff but still reasonably light roof panel. You can use a a mix of carbon kevlar or twaron down to personal preference.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Zemoleiro
Z
Forum Guru (56 reputation)Forum Guru (56 reputation)Forum Guru (56 reputation)Forum Guru (56 reputation)Forum Guru (56 reputation)Forum Guru (56 reputation)Forum Guru (56 reputation)Forum Guru (56 reputation)Forum Guru (56 reputation)
Group: Forum Members
Posts: 4, Visits: 20
Warren (Staff) - 1/23/2018 9:23:48 AM
A 5mm thick roof of solid laminate would be quite heavy.  You might want to consider the use of a structural core, such as 3mm Lantor Soric or 3D core.  Both are easy to infuse and will help product a stiff but still reasonably light roof panel. You can use a a mix of carbon kevlar or twaron down to personal preference.

Thanks a lot for your help. My idea is to use a Carbon Twill 200g. as first layer for a nice and clean look, the piece doesn't need to have 5mm. thick, I only want that it can resists to hard impacts or if the UTV capsizes doesn't crack.