Treated Carbon or Graphite fibres.


Author
Message
Umesh Marathe
Umesh Marathe
Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)
Group: Forum Members
Posts: 2, Visits: 3
Does easy composites supply treated carbon or graphite fibres/fabric?

Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
What kind of treated fibres do you mean? Some fabrics have special coatings for certain applications and almost all carbon fibre will have a sizing added to the fibre during manufacture.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Umesh Marathe
Umesh Marathe
Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)Forum Member (29 reputation)
Group: Forum Members
Posts: 2, Visits: 3
Warren (Staff) - 1/12/2018 4:53:32 PM
What kind of treated fibres do you mean? Some fabrics have special coatings for certain applications and almost all carbon fibre will have a sizing added to the fibre during manufacture.

I mean surface treatment like oxygen nitrogen plasma, etching by HNO3 acid on bare carbon fibres. We need such kind of treated fibres.

Warren (Staff)
Warren (Staff)
Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)Supreme Being (37K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
Unfortunately we do not have any fibres etched in that way.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search