Hello friends,

i am currently working on a project where we are manufacturing CFRP Parts with vacuum assisted RTM process. We are using infusion resin with infusion hardener (HP Textiles (HP-HE3000RI-30) / HP Textiles (HP-HTE300RI-9)) and Semiperm Monofilm R&G Release Agent. We are experiencing weird white spots inside of the part after curing of the resin and arent able to fix them. The wierd thing is, that we have these white spots very concentrated at a few positions of the part. The rest of the resin inside the resin pot is clear!  What could be the problem? This is how the process looks like:

1) Inserting preform into the tool
2) Closing of the tool
3) Vacuuming of the tool
4) Injecting of the resin with 0,7 bar injection pressure
5) Wait 2 days until resin is cured
6) Open the tool

I have added a picture inside of my post. I hope you can help.

Thank you very much for your potential help,

All the best, Nik


Reply
oekmont
oekmont
Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)Supreme Being (4.8K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
what type of pump are you using? what do the specifications say how much pressure it can reach?
30mbar happens to be the boiling point of water at room temperature. If you got a moisture problem, the pressure stops at this point during evacuation. Because of this, I degas at least down to 6mbar, at wich the boiling point is at 0°C. And during infusion, I try to maintain a slightly higher pressure, around 6-7 mbar, to prevent further degassing.

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
tsombnik - 7 Years Ago
Warren (Staff) - 7 Years Ago
tsombnik - 7 Years Ago
fibernoob - 7 Years Ago
tsombnik - 7 Years Ago
fibernoob - 7 Years Ago
oekmont - 7 Years Ago
tsombnik - 7 Years Ago
oekmont - 7 Years Ago
tsombnik - 7 Years Ago
oekmont - 7 Years Ago
tsombnik - 7 Years Ago
oekmont - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search