I just finished a split mold, made of High temp gelcoat + putty reinforcement
Before completing the second halve, I applied 6 easylease coats on the first halve of the mold and the pattern.
I left the mold to cure.
Can I let the mold 5 days before separating the two halves ? Will the easylease still work in 5 days . I know this is semi permanent release but I was wondering if it had a limit in time.

Thanks

Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
It is no problem. I often leave parts for several days or weeks prior to demoulding, to ensure the resin is well cured and reduce print-through. 
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Tony2125 - 8 Years Ago
oekmont - 8 Years Ago
Tony2125 - 8 Years Ago
Hanaldo - 8 Years Ago
Matt (Staff) - 8 Years Ago
Tony2125 - 8 Years Ago
Matt (Staff) - 7 Years Ago
Tony2125 - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search