By Tony2125 - 12/28/2017 1:07:30 PM
I just finished a split mold, made of High temp gelcoat + putty reinforcement Before completing the second halve, I applied 6 easylease coats on the first halve of the mold and the pattern. I left the mold to cure. Can I let the mold 5 days before separating the two halves ? Will the easylease still work in 5 days . I know this is semi permanent release but I was wondering if it had a limit in time.
Thanks
|
By Tony2125 - 1/4/2018 11:21:29 AM
No problem Matt All worked fine when I opened the mold 5 days later. Really happy with the result
|
|