Hi Tony,
Just checking in on the support forum over the Christmas break; I can see that you've been well looked after by oakmont and Hanaldo on this one; they're both right that you should be fine to come back to your Easy-Leased part several days later without any problems at all. If you're ever unsure then you can always add one extra application of Easy-Lease at least 1 hr before you lay up but we wouldn't expect any problems either way. One time when we would recommend re-application is if you're pulling the mould out of storage where it's been for months or years, in this case it would certainly be recommended to re-apply, just to be sure that so contamination from storage has interfered with the release agent.
All the best and enjoy your New Year.
Matt
Matt Statham Easy Composites / Carbon Mods - Technical Sales
|