I just finished a split mold, made of High temp gelcoat + putty reinforcement
Before completing the second halve, I applied 6 easylease coats on the first halve of the mold and the pattern.
I left the mold to cure.
Can I let the mold 5 days before separating the two halves ? Will the easylease still work in 5 days . I know this is semi permanent release but I was wondering if it had a limit in time.

Thanks

Replies
oekmont
oekmont
Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)Supreme Being (6.6K reputation)
Group: Forum Members
Posts: 550, Visits: 27K
Absolutely yes. Semi permanent means that it is possible (but not really recommended) to do several parts without applying the release agent between the cycles.
There is nothing like a time limit for any release agent I know of. But usually you want to make your part (or mold) reasonably soon after applying the release agent, to prevent the mold from catching dust.

Tony2125
Tony2125
Supreme Being (195 reputation)Supreme Being (195 reputation)Supreme Being (195 reputation)Supreme Being (195 reputation)Supreme Being (195 reputation)Supreme Being (195 reputation)Supreme Being (195 reputation)Supreme Being (195 reputation)Supreme Being (195 reputation)
Group: Forum Members
Posts: 12, Visits: 59
Ok , thanks for clarification
I have never been in this situation before , but this time I will leave home and the mold is not fully cured... so I hope this will work fine to open the mold when I will be back in 5 days
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Tony2125 - 9 Years Ago
oekmont - 9 Years Ago
Tony2125 - 9 Years Ago
Hanaldo - 9 Years Ago
Matt (Staff) - 9 Years Ago
Tony2125 - 9 Years Ago
Matt (Staff) - 8 Years Ago
Tony2125 - 8 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search