+x Kimberley1985 - 1/24/2018 11:59:20 PMHello I’m not sure how to write a question of my own, so apologies for jumping in here! I have done a penny table and have used epoxy resin and hardener on top, however in some places it is very tacky, and some places also look wet underneath the cured resin. what do you advise I do to rectify this? Also can I re resin just the areas in question or would I need to re resin the whole lot again? Any help would be greatly appreciated, thank you so much Kim x