I've made some basic trim pieces and have had good success, now I want to try this door pull for my car.  Where would you recommend I divide the mould sections?   I'm guessing this will need to be 3 pieces, correct?  Any help greatly appreciated.  



Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
The screw block on the rear would almost certainly need to be bonded on separately, perhaps a piece of suitable plastic cut to shape or even make a mould and resin cast a block with a small flange around it to increase the bonding surface area and hence bond strength.


Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant