Hi guys,

quite a while ago I came across the MTI hose, developed in Germany. A regular spiral tube (albeit a larger diameter) covered in an air-permeable membrane that is impervious to resins.

Question is, are any of you familiar with this product? They promise cosmetic, pinhole-free surface, without the need for catchpot and continuous vacuum. Was just curious if easycomposites or some of the other pros out there have any experience and if its worth giving a try, looks interesting.

Cheers
Reply
olorin
olorin
Supreme Being (75 reputation)Supreme Being (75 reputation)Supreme Being (75 reputation)Supreme Being (75 reputation)Supreme Being (75 reputation)Supreme Being (75 reputation)Supreme Being (75 reputation)Supreme Being (75 reputation)Supreme Being (75 reputation)
Group: Forum Members
Posts: 9, Visits: 51
Warren (26/07/2012)
to add, surely a better design would be to have such a hose with slightly bigger pores to slow down the resin going into the vacuum line rather than stop it.  Then you would have the advantages of the resin flow being pulled to the edges all round on a complicated part (path of least resistance is through empty laminate rather than wet laminate) but still be able to ensure an even vacuum all over as the small resin flow into the vacuum line would still mean an even vacuum can be pulled all over and still allow any tiny bubbles from the resin to be drawn out.


I agree totally with the Supreme Being.

In fact, I would think it an unwise choice to disagree with a Supreme Being. Smile
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
baja_patient - 14 Years Ago
Dave - 14 Years Ago
     ...
baja_patient - 14 Years Ago
r0bsk1 - 14 Years Ago
Warren - 14 Years Ago
sebgron - 14 Years Ago
fgayford - 14 Years Ago
Designbikes - 13 Years Ago
Warren - 14 Years Ago
olorin - 14 Years Ago
Warren - 14 Years Ago
olorin - 14 Years Ago
baja_patient - 14 Years Ago
Warren - 14 Years Ago
Designbikes - 14 Years Ago
baja_patient - 14 Years Ago
sebgron - 14 Years Ago
DD-Compound - 13 Years Ago
Shaneer22 - 13 Years Ago
Warren (Staff) - 13 Years Ago
DD-Compound - 13 Years Ago
carbonfibreworks - 13 Years Ago
Zero Mass Motorsports - 13 Years Ago
baja_patient - 13 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search