I want to make a mould of these 2 repaired end caps from carbon, i never did a shape like this deep and would like to know what is the best way to go?

Put them flat on a plate and mould or maybe a 2 piece?



thanks

Edited 8 Years Ago by Thomb
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
That doesn't look like it would release if on a board as a one piece mould.
May have to be a split mould?

One piece mould would be nice and easy though. You should blank off the smaller open end and mould right across this area.





Edited 8 Years Ago by Fasta
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search