Hi all.

I would like to place a logo on a carbon part without having to  simply stick a decal over the finished part.

I was thinking of covering the  logo(sticker) with clear but I will then get a raised section of the logo.

What are the methods other than just sticking a logo above the part  ? 



I have seen some logos on parts that seem perfectly "painted".  (see image as an example) .



EVR Ducati Hypermotard 1100 Carbon Fiber Air Box 

http://www.kmmotorcycleparts.com/files/2688938/uploaded/800-EVR105-11.jpg
Hanaldo
Hanaldo
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Well most things like that will be done with plenty of wet-sanding to remove that raised edge around the sticker. I'd wager that part has been sprayed 2-3 times. 

However, I've done it before with infusion. If you can work out a way to get the positioning correct (obviously the sticker needs to go into the mould with the surface down, which means you can't stick it in place), then you can put the sticker into the infusion stack and it will just be part of the laminate. This is my preferred method, but it is difficult to make sure the sticker stays where you want it. Nothing worse than going through all that effort only to find your sticker is on an angle when you demould. 
rmaddock
rmaddock
Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)
Group: Forum Members
Posts: 17, Visits: 1.5K
What about transfers rather than stickers? They're very thin.
For example https://www.craftycomputerpaper.co.uk/decal-paper-c553/inkjet-water-slide-decals-c562/inkjet-water-slide-decal-paper-p11228

Further to the above.....you might be able to then clear coat over them....but you'd have to experiment. I've had these and sealed them with an acrylic spray varnish.
Edited 9 Years Ago by rmaddock
davro
davro
Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)
Group: Forum Members
Posts: 300, Visits: 2.2K
I clear coated over the top of some stickers for a rc bodyshell once and like Hanaldo said plenty of wet sanding.
Build thread is here http://www.talkcomposites.com/13092/RC-Car-Touring-Body-110-Scale

Also, I really like the way marsh powerhouse fab does his very suttle logo on his carbon bonnets
https://www.instagram.com/p/BRWUAVlAJpL/?taken-by=marshpowerhousefab

I'm planning soon to airbrush on a small design British flag and driver name to my carbon scuttle, and then a few layers of clear coat.

Might give the water slide ink jet method a try as I don't have access to a vinyl printer anymore.



David Stevens
YouTubeComment | Rate | Subscribe
Instagram

Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale


Edited 9 Years Ago by davro
ChrisR
ChrisR
Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)Supreme Being (2.9K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
It depends on the thickness of the sticker, you can get it as thin as 0.05mm thick, I dare you to find a ridge!!
davro
davro
Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)
Group: Forum Members
Posts: 300, Visits: 2.2K
I played around with some waterslide inkjet paper and some clear coat to seal the ink, after rmaddock mentioned about water slide.

It's a fun technique for making decals and works really well for transparent decals as white becomes transparent and it looks quite nice with carbon showing through Smile


Prefer the all black look (image is a bit dark)


Just need to put the final clear coats on the scuttle now ...



David Stevens
YouTubeComment | Rate | Subscribe
Instagram

Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale


Edited 9 Years Ago by davro
rmaddock
rmaddock
Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)Supreme Being (152 reputation)
Group: Forum Members
Posts: 17, Visits: 1.5K
Nice.
I think you can get two types of transfer paper, like you've got with a transparent base and also one with an opaque base.......I hunk.
Fasta
Fasta
Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)Supreme Being (4.1K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
Are these waterslide decals also clear coated on your parts too?

I recently got some waterslide materials but was thinking to try and put this in my laminate first behind the in mould coating. What do you think about that?

Do you think a logo could be slid off the sheet using resin instead of water, then place straight into the mould?





davro (20/05/2017)
I played around with some waterslide inkjet paper and some clear coat to seal the ink, after rmaddock mentioned about water slide.

It's a fun technique for making decals and works really well for transparent decals as white becomes transparent and it looks quite nice with carbon showing through Smile


Prefer the all black look (image is a bit dark)


Just need to put the final clear coats on the scuttle now ...





Edited 9 Years Ago by Fasta
davro
davro
Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)Supreme Being (2.7K reputation)
Group: Forum Members
Posts: 300, Visits: 2.2K
I am in the process of putting on the final layers of clear coat over the water slide decal.

Not sure about sliding one into the mould as the water slip stuff is on the backing of the paper and you would want the face or the front of the decal to be on the inside of the mould if you get what I'm saying ...

I think you might have trouble slipping of the decal using resin as they are very delicate and susceptible to stretching and deforming the water makes it very slippery and easy to handle and slip into place also the material needs to dry in place else it will be damaged or distorted when applying the laminate. Though you might want to run a few tests with some small decals as I might be completely wrong with my thoughts Smile



David Stevens
YouTubeComment | Rate | Subscribe
Instagram

Composite Projects
Body Package for Dax Rush
RC Car Touring Body 1/10 Scale


David Vale
D
Supreme Being (88 reputation)Supreme Being (88 reputation)Supreme Being (88 reputation)Supreme Being (88 reputation)Supreme Being (88 reputation)Supreme Being (88 reputation)Supreme Being (88 reputation)Supreme Being (88 reputation)Supreme Being (88 reputation)
Group: Forum Members
Posts: 10, Visits: 109
I am trying to look at an easy method of applying decals to an aircraft panel. There are lots of them. I did discuss this with Paul the other month but there seems to be no definitive way of doing this. I am currently looking at waterslide and the suggestion was applying this to the mould with a minimum tack before infusion. This could be prone to misalignment in the process. Using. Vinyl stencils seems a problem as the letters need to be small and precise alignment and then will require a silkscreen print to fill the vinyl stencils after removing.
My thoughts are would it be better to create the panel, apply waterslide decals and then use an XCR resin coat to seal them forever in resin. Anyone experience of this and any advice would be appreciated.

Retired - Thank heavens, and still don't have enough time during the day
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search